Conductor Failure Investigation Checklist

Record the defect, material construction and process conditions, then use targeted inspections to narrow the possible causes.

Audience
Quality engineers, reliability engineers, supplier quality engineers
Purpose
Input: affected/reference lots and process records. Output: evidence for a cause investigation.
Conductor Failure Investigation Checklist: project record — open worksheet

Record your project requirements and observations, then download or include them in an inquiry.

ItemInformation / unitsYour input
Material and symptomMaterial form, affected lot and observed symptom
Control lotUnaffected lot and same-condition comparison
Evidence and hypothesisPhoto, measurement and potential cause to investigate
Next checkControlled repeat, result and conclusion
Other formats and preview
Save or restore a draft

Drafts stay in this browser. Clear inputs also removes the saved draft.

Worksheet version: RT-RFQ-WORKSHEET-1.

Investigate the observed symptom

Use possible causes as hypotheses; compare affected and unaffected samples.

Scroll horizontally to view all columns.

Symptom and formPossible causesNext checkEvidence needed
Layer separation in clad wire/stripInterface preparation, process variation, severe forming or test damageCompare layer continuity before/after the operation; inspect reference lotCross-section, lot/process history and forming/test conditions
Cracks, burrs or coil-feed problemsCondition, edge damage, tooling, tension or packingCompare incoming material with formed/handled samplesDimensions, temper/strength records, edges, spool and settings
Raised resistance or a local hot jointSection change, contact resistance, oxidation or damageMeasure conductor and joint separately under the same conditionsCurrent/temperature record, voltage drops, joint/section images
PV low peel or cell damageWetting, coating, contamination, cell surface, profile or handlingRun controlled cell/ribbon lot comparisons; classify the failure locationCell/ribbon lots, coating data, peel method, profile and EL images

Keep the investigation traceable

Assign an owner and evidence requirement before closing a hypothesis.

RecordRequired detail
DefectLocation, occurrence rate, photos, sample/lot and process stage
TestAgreed method, specimen, conditions, result and project acceptance requirement
ComparisonAffected versus reference lot with variables held constant